Jul 12, 2022

Technology Of Producing Steel Castings Furan Resin Sand

Leave a message

Furan resin sand is one of the fastest developing casting processes in the past 20 years. Castings produced by furan resin sand have accurate size, smooth surface, clear edges and angles, low reject rate, and can save modeling time, improve production efficiency, improve working conditions and production environment. For furan resin sand casting production technology, I think, no matter from the technical management and quality management and production management should control the application of furan resin sand in foundry production and quality, and stressed that only by strengthening the site management and process control, gradually improve the staff's quality consciousness, improve the quality of the operation of the production process, change passive management to active management, In order to effectively ensure the internal quality and surface quality of products. It is emphasized that the technical personnel and management personnel should have the consciousness of innovation and service, and timely solve and deal with the problems in the production process, so as to continuously improve the technical level and management level of the enterprise.

1. Control the materials used in modeling

1.1 Selection of resin Selection of resin will have a direct impact on casting quality. If the resin chosen is not good, it will increase the amount of resin, but also affect the quality of sand, leading to more castings waste. Therefore, the selection of raw materials, can not only be combined with the implementation of the technical standards of the enterprise, but also need to be familiar with the production process of the enterprise, production equipment, and as far as possible to test a series of indicators of resin, or the experience of similar production enterprises for reference.

1.2 The composition of the original sand is scrub sand, washed sand and ordinary sand. Because scrub sand contains very little mud, it can reduce the waste of resin and needs to be selected first. Again, it is to choose washed sand, but the raw sand without treatment can not be applied. The selection of sand type, one is to choose the original sand with relatively low angular coefficient as far as possible, and the other is to choose the nearest sand to reduce the cost of transportation.

1.3 Choose other raw materials other raw materials have coating, release agent, etc., the selection of these raw materials, should consider its quality and match with important materials, such as easy to transport and procurement. These materials can affect the cost of casting.

1.4 Adding reasonable curing agent and resin by effectively controlling the hardening characteristics and sand temperature, adding curing dose is best 30% to 50% of the amount of resin, too low or too high curing agent is difficult to achieve higher hardening characteristics of sand. Because the temperature difference between summer and winter is relatively large, it should be combined with climate factors to change the brand of curing agent in real time, to avoid the quality problems caused by improper application of molding core.

1.5 is reasonable in the application of furan resin sand mold strength and the production process, along with the increased amount of resin and improve the strength of resin sand, after more than the corresponding limits, however, to further improve the strength of will not significantly, sand mold core strength is too high the adverse effects on the production of steel, affect the shrinkage of steel casting, casting hot crack more easily. Hardening characteristics of furan resin, which should be effectively controlled, the strength of sand mold just need to conform with process control, to protect steel production needs, generally need to make sure that type (core) under the pouring and type, core, and the process of handling strength enough not to be damaged, with the process type, the shape and size of (core), generally speaking, The final strength of moulding sand is 0.6MPA-0.8mpa, while that of core sand is 0.8MPa-1.0mpa.

1.6 Controlling sand temperature Hardening characteristics of furan resin self-hardening sand are closely related to environmental temperature and sand temperature, especially sand temperature directly affects hardening. Reasonable control of sand temperature can reduce the use of curing agent, achieve better hardening characteristics, and reduce sulfur permeability of castings. Control sand temperature regulator, usually need to control the sand temperature of 20℃ - 30℃.

2. Effective control of the whole production process

2.1 Ensure the tightness of the core When making the core and molding the furan resin self-hardening sand, be sure to ensure that the core is tight, otherwise, the casting is prone to lack of sand sticking. It is forbidden to release sand through sand mixing machine. It is finished after scraping. In core making and modeling, with the help of appropriate tools and the same as the sand mixing machine filling route and in the process of sand tamping, for the location of the more difficult to operate, be sure to tamp, and ensure the uniformity of core compaction.

2.2 The production of steel castings with coating is closely related to coating. In combination with furan resin sand, a better casting surface can be achieved, and sulfur infiltration on the casting surface can be effectively controlled to avoid sand mold infiltration into molten steel, prevent the gas produced by sand mold core, and avoid defects such as porosity and sand sticking. When resin sand is used to produce steel castings, various forms of paint can be applied. Coating aggregate needs to have better sand resistance, coating needs to have higher suspension and brushing, as well as higher cracking resistance and high temperature strength. A, not drying alcohol-based coating technology: with the help of alcohol-based zirconium coating, after brushing ignition combustion fully, do not need to be dried separately, can directly buckle box pouring. B, drying water-based coating surface technology: with the help of chromite ore powder, zirconium powder, and some other composite aggregate water-based coating, coated to reach 180 ℃ - 200 ℃ temperature channel drying kiln to dry, drying time is 45 minutes - 60 minutes.

2.3 Improvement of sand core concession on the basis of ensuring production performance and corresponding strength, the amount of resin added increases, the amount of resin added will affect the strength of sand, if the amount of resin added is reduced, then the overall strength of sand will be reduced, and then the concession of sand can be improved. For the core that blocks the shrinkage of the casting, concessional materials should be put into the sand mold and sand core, such as resin sand block, nylon rope, and straw rope, and so on, so that the sand core can be improved. As far as possible to reduce the sand-iron ratio of the casting, because the furan resin self-hardening sand casting has a very poor thermal conductivity, so reducing the sand-iron ratio can make the sand mold yield and improve.

2.4 Core exhaust because of the furan resin self-hardening sand sand yield poor, high temperature strength, large gas, so easy to crack and porosity, should solve this problem, in addition to the addition of curing agent and resin amount of control, be sure to pay attention to the core exhaust and concession. Sand box plate with sand box plate exhaust, because the resin sand has good fluidity, sand box vent is not suitable for too large, but the number of sand box vent needs to be appropriately increased. Exhaust holes are more tied in the sand model (core), in the sand model (core) before hardening, a certain amount of exhaust holes will be tied up, to ensure smooth gas. When scraping the terrain, the embedded air pipe or air outlet groove can be scraped out, and then the gas can be smoothly discharged after the casting of the sand core. In the core will be out of the pipe embedded, the core under good, with the help of ventilation rope out of the type, connected with the atmosphere, to ensure that the core can be unobstructed exhaust. When pouring, the gas is ignited in real time so that the gas generated by pouring can be discharged from the cavity in time.

Struggling with low sand Casting efficiency?

With 30 years of Furan Resin Sand Casting experience,

we offer efficient solutions to boost productivity, reduce costs,

and maximize your benefits!

Phone Number(Whatsapp)

+8618765972210

E-mail

cassie@besttechmachinery.com

resin sand molding line 1288

 

 

 

Send Inquiry